MAX Cool process

Available as an option in Master M 355.

MAX Cool is a short arc MIG/MAG welding process that is designed for root pass welds and sheet metal (thin sheet) applications. It’s fully current-controlled welding process. MAX Cool does not require the use of a separate voltage sensing cable.

MAX Cool is suitable for all welding positions and provides a smooth arc, reducing spatter.

>>  To take MAX Cool into use, press the control panel's welding process button and select MAX Cool.

>>  To adjust the wire feed speed, in the Main view, turn the left control knob. The adjustment's effect on the plate thickness is also shown.

>>  To fine-tune the heat output, in the Main view, turn the right control knob.

MAX Cool supports these filler wire and shielding gas combinations:

Fe solid & Ar + 8…25 % CO2 (1.0 mm, 1.2 mm)
Fe solid & CO2 (1.0 mm, 1.2 mm)
Ss solid & Ar + 2 % CO2 (1.0 mm, 1.2 mm)
CuSi3 & Ar (1.0 mm)
CuAl8 & Ar (1.0 mm).